Terbium

Electrochemical properties


Electrode potentials


e° (V): Tb(IV)/Tb(III): 3.1 [1]
Tb(III)/Tb: -2.31 [1]


Conductivity


Electrical resisitvity (μΩ·cm): 116.00 (20 °C) [2]
107.00 (25 °C) [2]
Thermal (W/m·K): 11.1 (27 °C) [3]